Paint-ready or wallpaper-ready plaster?
If the wall is getting latex or wall paint, you need paint-ready (sausklaar) plaster; if it is getting thick wallpaper, wallpaper-ready (behangklaar) is enough. Paint-ready is smoother and flatter, because paint shows every unevenness. The trade prefers the quality groups of the Technisch Bureau Afbouw (TBA), because 'sausklaar' and 'behangklaar' lead to disputes.
Rather not work it out yourself? Ask for a free quote, in English, with covering and cleaning up included.
Get a free quoteUpdated on · Edited by: Samir El Ouariachi, painter and plasterer
What the difference means in practice
Paint and latex lie over the wall like a thin skin. Every bump, every trowel mark and every little hole shows through afterwards, especially when light falls along the wall. Wallpaper, certainly thicker wallpaper, covers small irregularities. That is why wallpaper-ready work can be less smooth, and why it is cheaper.
Not sure whether the wall will ever be painted? Then choose paint-ready. Going from wallpaper-ready to paint-ready later means another coat of plaster, so covering up, plastering and drying all over again.
The TBA groups: what the trade agrees on
The Technisch Bureau Afbouw divides interior plasterwork into seven groups, from 0 to 6. Its table card 'Oppervlaktebeoordelingscriteria stukadoorswerk binnen' (surface assessment criteria for interior plasterwork, March 2018) sets out which finish suits each group.
- Group 0: very smooth, for a gloss paint finish. A test area is mandatory.
- Group 1: smooth, for a matt paint finish, vinyl wallpaper or glass fibre wallcovering. This is what most people call 'sausklaar' (paint-ready). A test area is mandatory here too.
- Groups 2 and 3: smooth enough for thicker wallpaper or decorative plaster with a coarser grain.
- Group 6: local repair, with no requirements for flatness. According to TBA, this is what is often called 'behangklaar' (wallpaper-ready), and only thick wallpaper suits it.
How to put it in your quote
Don't just ask for 'sausklaar': have the TBA group written into the quote and agree on a test area, a section of wall that serves as the benchmark for the rest. Judge the work without raking light, so not with a lamp or sunlight shining at an angle along the wall. That is how TBA prescribes it too, and it prevents disputes afterwards.
Sources
- TBA table card 2, Oppervlaktebeoordelingscriteria stukadoorswerk binnen (March 2018, in Dutch), checked 30-09-2026
- SchildersVAK, TBA is klaar met 'sausklaar' (23-02-2021, in Dutch), checked 30-09-2026
Also asked
Can I put latex paint on wallpaper-ready plaster?
You can, but the irregularities will show. For a crisp result, a thin coat of plaster goes over it first to make the wall paint-ready.
Is paint-ready more expensive than wallpaper-ready?
Yes, because more time goes into getting the wall smooth and flat. Price guides give higher prices per m² for paint-ready work than for wallpaper-ready; see the ranges with sources on the prices page.
What is a test area?
A section of wall that you approve together with the plasterer as the example. The rest of the work is compared against it. For TBA groups 0 and 1, a test area is mandatory.